Cryogenic Liquid Cylinders- Safe Lifting Method


A few weeks ago we discussed some of the potential hazards and risks associated with lifting liquid cylinders to elevated locations along with ways not to lift them. It is agreed among all manufacturers that the handling ring around the top of a liquid cylinder is not to be used as a lifting point. While some instruction manuals show cryogenic liquid cylinders being lifted by the holes in the handling ring support brackets this is not a universally recommended practice. This is especially true regarding full cylinders being lifted overhead. The risk of lifting any liquid argon, oxygen or nitrogen vgls by the support brackets are that:

a) It is unlikely if you know the specific cylinder you are lifting is one with supports designed for lifting;
b) The liquid cylinder supports could have been weakened over time by being bent and straightened or through metal fatigue or corrosion.

In any case- the support brackets can tear away from the vessel allowing it to drop. A liquid cylinder full of product that is dropped from an overhead location is a clear hazard.

So- What are the options?

1) Consider running feed lines up from your vessel to the work area first and keeping all liquid containers at ground level;
2) If the distance from the ground to a work area is prohibitively long then use a safe carrier to raise the vessel to the area needed.

A photograph of an enclosed carrier for lifting liquid cylinders is shown. These can also be fitted with lifting eyes on all four corners for 4-point lifting. Be sure that whatever you use that the device is regularly inspected for damage or corrosion and that any lifting cables are in-spec for the intended purpose.




Thursday, February 19, 2009

Is Microbulk Cultural?


Seven or eight years ago U.S. Manufacturers were told that there would be no real reason for them to do much in the way of 250-500 gallon vertical bulk tank production. Reasons given included plentiful stocks of used equipment and the inability of suppliers to economically justify small volume cryogenic liquid deliveries. Yet, During the past few years, sales of microbulk vessels in the 1000 to 2000 liter range have been strong. These are the same sized vessels just packaged differently.

This might be ironic except for the fact that “Nature abhors a vacuum.” And- just because a major producer of liquid oxygen, nitrogen and argon has a business model that focuses their efforts on deliveries of 1500 gallons or more does not preclude the need of users. Posed with the question of how to fill the gap from liquid cylinders to 1500 gallon bulk tanks one producer eloquently responded “That’s what distributors are for.” And in the U.S. this has proven largely true.

Interestingly enough, though, I was informed that some of the same companies who have 1500+ models in the U.S. are actively involved in establishing a microbulk presence in Europe and Asia. Part of the answer given for this is a cultural aversion in other countries to soliciting a competitor’s clients for nearly identical services. For example- If Manufacturer X is buying 20-30 liquid nitrogen cylinder exchanges per month then it might be considered unseemly for a competitive supplier to come in and offer to provide the same service at a lower rate. But- A competitive supplier who offers the same liquid in a different package is offering an alternative that changes the rules of the game.

I’m told it would still be “unseemly” to go out directly soliciting microbulk business as an alternative, but there are means of finessing the approach so that the client calls the supplier to initiate discussion. Economic presentations at trade shows, article publication, web posting and general advertisement all become fair game along with referrals from other happy clients. Overall, this is sort of a retail walk-in approach to engaging clients vs. a more active direct approach in the U.S.


Thursday, February 12, 2009

Vacuum Rupture Disk D- CSI Outer Leak

Another client met me at the door saying, “Your timing is perfect. Come back to the plant and see what you can tell us about this freshly rehabbed vessel that we are having some trouble filling.” The problem was apparent from about ten feet away. We walked on up to the vessel and found a neat hole (about welding wire diameter) that went through the plastic rupture disk cover, the “Do Not Remove” warning and apparently through the rupture disk. The plastic cover and label were removed to reveal the expected “sucked in” rupture disk. This was obvious tampering and one of the few times I’ve seen it done through the rupture disk cover.

Vacuum rupture disks plastic covers are put on cryogenic liquid cylinders both to prevent tampering and to protect the very thin disk material from welding and cutting sparks and corrosion. A supplier who is able to consistently assure that all liquids go out with rupture disk covers in place is both protecting their assets and providing a ready visual indicator for drivers to help with spotting potential problems.

Many of the liquid oxygen, argon, and nitrogen bottles that come in with blown rupture disks are clearly tampered with. Spotting problems at the user site and documenting them helps with the possibility for recovering the cost of repairs for damages.

A lot of people believe that “if you take care of the nickels the dollars will follow.” Here is a case in point.

Thursday, January 29, 2009

Rehab Compared to New- Questions


Thanks to all of you who are sending in great questions including these today:

Q: Do rehabilitated liquid cylinder vacuums last as long as the vacuums on new cylinders? I have some rehabilitated cylinders that have been in service 3-5 years, and have a bad vacuum. I know there are a lot of variables, mostly cylinder handling.

A: You are right. There are a lot of variables. It is actually possible for a rehab vacuum to be better than new depending on the quality of the original vessel manufacturing and first vacuum pull. Heating, time and vacuum pump strength make huge differences in performance. Generally, though, rehabs are done on older vessels so they will be less pristine after rehab than when brand new. They might also have experienced damage, corrosion and introduction of moisture into the annulus. All these factors can affect long-term performance and reinforce the importance of both manufacturing and service quality and process integrity.

Q: I also noticed that, after rehab, there are some welded patches on the cylinders. Do these patched areas cause some new leaks just because a patch cannot be as good as solid material?

A: If the welds are done properly they should not be a new source of leaks (with “properly” being the key word). Leaks are more frequently the results of damage, corrosion or bad metal integrity.

Wednesday, January 21, 2009

Customer Vacuum Question- Part 1


A client called yesterday with a couple of good questions. Here is the first:

“Do you pull vacuums on liquid cylinders when you rehab them and if so to what level?”

Yes. Cryogenic liquid oxygen, argon and nitrogen have very low boiling points. Nitrogen for instance boils (converts to gas) at
-195.8 °C or -320.44 °F. Keeping argon, nitrogen and argon cold enough to maintain them in a liquid state requires specialized vacuum insulated containers. Cryogenic liquid cylinders are double walled vessels with a super-insulation wrapped inner container that holds the liquid and is inserted into a slightly larger outer vessel. The annular space (annulus) between the two vessels is used to insulate the liquid. After both vessels are sealed leak tight a vacuum is pulled on the annulus to remove virtually all atmospheric molecules and impede the transfer of energy.

To be an effective insulator this vacuum has to be pulled to very low levels. Leaks will result in a loss of vacuum and the need for rehab. West Cryogenics performs a helium mass-spec leak investigation at rehab to check for molecular level leaks. Then the vacuum is pulled to < 10 microns. The vacuum pull is done in two phases (hot and room temperature) to assure all moisture and other stray molecules are removed. A final inspection is performed after refinishing and other testing to verify that the vacuum has not risen due to latent moisture or a leak that needs to be found and repaired. If final inspection shows a weakening of the vacuum then the liquid cylinder goes back to mass-spec and vacuum restoration.